Rapid RH L6 products are launched to enhance the ease, quickness, and data integrity that made the Rapid RH concrete moisture testing system the tool of choice for professional floor covering installers and inspectors around the world:
- Rapid RH L6 Total Reader® with Bluetooth® and ambient Temp/RH sensor
- Rapid RH L6 Smart Sensor with increased responsiveness in high RH concrete
- DataMaster™ L6 free smart device app with improved visual mapping
Wagner Meters launches the specialized C555 Electronic Concrete Moisture Meter as a tool for improving the efficiency of in-situ concrete moisture testing as described in ASTM F2659.
The Orion 950 wins the Association of Woodworkers and Furniture Suppliers (AWFS) 2019 “Visionary Award” for its multipurpose functionality and exclusive ability to be calibrated by the user.