How Moisture Can Ruin Your Decorative Concrete
From majestic castles to modern architectural masterpieces, concrete has been a foundation of construction for centuries. In today’s contemporary spaces, decorative concrete stands out not just for its structural benefits but also for its aesthetic value. It can transform a plain surface into an elegant masterpiece when perfectly executed.
However, like every work of art, it demands precision and care. One of the prime adversaries of decorative concrete is moisture. If left unchecked, the silent eroder and moisture can tarnish the beauty and strength that decorative concrete imparts to a space.
In this article, we delve deep into understanding the relationship between moisture and concrete and how to protect your decorative flooring from its insidious effects.
- Signs That the Finish Was Applied at the Wrong Time
- Why is My Concrete Turning White?
- Concrete Stains: Reactive and Non-Reactive
- Concrete Sealers: Water-Based and Solvent-Based
- Avoid Water Stains on New Concrete with Accurate Moisture Testing
- Each Project Requires a Unique Assessment of Proper Moisture Conditions
Excess moisture doesn’t just evaporate; it takes your design with it. You can preserve your design and the concrete with proper moisture testing before stains and sealers are applied.
Beauty and strength converge in decorative concrete. Like a good acid stain, they fuse together to create a durable, pleasing floor that literally becomes the foundation of its space and atmosphere. Achieving the desired result requires that you consider a number of variables for the specific concrete stain and sealer combination you select.
One of the most important variables that need your attention is the moisture content in the concrete at the time the stain and sealer are applied. Moisture in concrete can come from two main sources. The first is the volume of water used to mix the cement into concrete.
Second, external sources of water may be an issue, such as water that can migrate from the ground to the concrete slab in the absence of a vapor retarder.
Both evaporating water and pooled water can interfere with a concrete stain or sealer.
Signs That the Finish Was Applied at the Wrong Time
The damage that excess moisture can do to your stain or sealer can look different depending on the amount of excess moisture and the type of stain or sealer used. Here are some common indicators that the stain or sealer was applied too soon – before the concrete had a chance to dry sufficiently:
Why is My Concrete Turning White?
Efflorescence is a white salty residue caused when too much moisture is moving through the concrete. As the concrete dries and its moisture rises upwards through the slab, it brings salts within the concrete to the surface as well. As lovely as the word sounds, efflorescence is rather unsightly.
Depending on whether or not the floor has been finished yet, efflorescence manifests in different ways. It can leave a white powdery substance on the concrete’s surface after staining but before sealing.
If the efflorescence gets trapped underneath a concrete sealer and/or certain water-based stains, it will look like stained white concrete floors.
Efflorescence can cause other stain or sealer failures, which are noted below.

Concrete Stains: Reactive and Non-Reactive
Reactive and non-reactive stains color the concrete in different ways, leading to different indications of moisture damage. In the case of reactive stains, the problems generally have to do with color variations.
- Undesirable color changes
- Lighter or uneven coloring
- Flaking and peeling
- Bubbling or blistering
- Dark spots
– The acid in reactive stains contains metallic salts that instigate a chemical reaction when they mix with the free lime in the concrete. This reaction provides the stain color, but when excess moisture exists, the salts or acids in some blue and green stains can turn brown or black.
The exact cause isn’t clear, but the most popular explanations attribute the undesired color change either to oxidation or a fungus, both of which can happen with excess moisture.
– Efflorescing salts in the presence of excess moisture will retard stain penetration, which interferes with the chemical process of the acid stain coloring the concrete.
The use of non-reactive stains in the presence of excess moisture gives rise to a different set of issues. Since a non-reactive stain colors the concrete by filling the concrete’s pores or by creating a film that sits on the concrete’s surface, typical moisture-related problems include flaking, peeling, bubbling, blistering and dark spots.
– an indication that the stain failed to bond with the concrete due to excessive moisture
– caused by moisture that can’t escape
– a sign of trapped moisture that can’t evaporate
All of these can cause concrete discolorations.
Concrete Sealers: Water-Based and Solvent-Based
Excess moisture can create several different problems when it comes to using sealers. The first one described here occurs when using a water-based sealer. The rest may occur when solvent-based sealers are applied in the presence of excess moisture.
- Powdery or white substance
- Greyish or cloudy spots
- Color whitens or “blushes”
- Cracking, chipping, peeling, or flaking
- Frothy foam
– The sealing agent evaporates faster than the water when there’s too much humidity, so they never bond together, leaving this substance behind.
– Moisture can lift the sealer from the concrete, which causes light to diffuse underneath the sealer (also called “sealer diffusion”), resulting in the appearance of discoloration.
– Too much moisture on the surface prevented the sealer from bonding, so it floats on the water instead.
– This is another consequence of moisture that can’t escape.
– The resin in a two-part solvent sealer bubbles when mixed with too much water, leaving a foamy substance.
Avoid Water Stains on New Concrete with Accurate Moisture Testing
As the concrete dries, moisture evaporates. Since a vapor retarder is typically placed underneath interior concrete slab installations, all of the moisture must evaporate by traveling upwards through the slab.
Furthermore, if the relative humidity (RH) in the concrete and the air around it are different, the concrete will either give off or absorb moisture. The volume of water to be evaporated and the rate at which it evaporates both impact when the concrete is ready to take a stain or sealer.
The many moisture-related problems described above can be avoided if the stain and sealer are applied when the moisture content within the concrete slab reaches an acceptable range – one that takes into account the specific moisture tolerance for the planned finishes.
By waiting until the concrete has dried sufficiently, you won’t be trapping excess moisture when applying the stain and sealer.
Conducting a moisture test beforehand is the only way to determine if the concrete is ready to be finished. One commonly-used moisture test in the United States is the calcium chloride test.
This test relies on an element (a salt compound) placed on the concrete’s surface to gauge whether excess moisture remains. The problem with this test is that it only measures moisture at the surface.
Because a moisture gradient (drier at the top, wetter at the bottom) exists within the concrete slab as it dries, the calcium chloride test does not provide an accurate representation of the true moisture condition deeper within the slab, nor does this test indicate the moisture that will later be seen at the surface as the slab moves toward a moisture equilibrium.
A far better test for evaluating the true moisture condition of the concrete is in situ RH testing. This test has been used for some time in Europe and is now becoming the standard in the United States due to the scientific evidence supporting its accuracy.

When RH probes are placed at 40 percent depth within the concrete slab (the correct depth for placement when the slab is drying from the top only), it has been demonstrated that the test results provide an accurate representation of the RH in the slab after it is sealed.
If the RH is too high for the finish’s tolerance, the finish may not live up to the expected visual and/or performance expectations.
While it is critical to choose the right test – in situ RH – for getting an accurate measure of the moisture level of a concrete slab, it is equally critical to know the RH readings that will be considered acceptable for applying a finish for your specific project.
Each Project Requires a Unique Assessment of Proper Moisture Conditions
The results of the RH moisture test must be evaluated against the moisture tolerance specified by the manufacturer for that exact stain or sealer. Pay particular attention to how permeable or “breathable” the finish is.
Epoxies are the least permeable, which means moisture trying to escape the slab is unable to do so, and if those moisture (RH%) levels are in excess manufacturer’s recommendations, these will be the most likely to cause damage.

Free Download – 4 Reasons Why Your Concrete Is Taking Forever to Dry
The manufacturers of the stain and sealer being used in your project have their recommendations, which must be considered. However, certain other factors, which may be unique to your project, should also be taken into account.
Here are some crucial variables to include when determining the acceptable RH range for your flooring finishes:
- age and thickness of the concrete
- grade of the slab
- any materials being used to prepare the concrete and the water contents of each
- ambient concrete drying conditions
- time available for the concrete to dry, including the time to dry between the stain application and the sealer application
Waiting to apply the stain and sealer until the polished concrete is ready takes planning and patience. However, the little bit of extra effort is more than worth it.
Achieving the perfect decorative concrete is a blend of art and science. As with all great endeavors, the devil is in the details. If left unchecked, the menace of moisture can lead to a cascade of issues that undermine the essence of decorative concrete – its beauty and durability.
Fortunately, these challenges are manageable with the proper precautions, tools, and a commitment to excellence. By understanding the unique moisture needs of each project and taking proactive measures like accurate moisture testing, we can preserve the integrity and beauty of our decorative concrete.
After all, the key to longevity in any craft, whether construction or otherwise, lies in understanding its nuances and preparing for pitfalls. So, before you embark on your next decorative concrete project, remember the mantra: test, assess, and proceed confidently.
Make sure to test your concrete flooring with the most accurate concrete moisture test.
Jason has 20+ years’ experience in sales and sales management in a spectrum of industries and has successfully launched a variety of products to the market, including the original Rapid RH® concrete moisture tests. He currently works with Wagner Meters as our Rapid RH® product sales manager.
Last updated on December 11th, 2024


I had an inground pool, cement pad and cement stairs all put in last Summer. Only the stairs were sealed so far, but I dislike the color (they ended up orange) so I used xylene to remove the seal and hopefully the color. A good bit of the color came off, but not all. Is there a tinted seal that I can use that can help blend my not orange pool concrete with my still sort of orange stair concrete without making everything orange?
Stacey:
I would reach out to a local decorative concrete supplier and ask for recommendations on this. Good luck.
I purchased my home here in Texas in July. I think it was Sept or Oct that I stained my patio. Recently I am getting condensation on the stained portion of the concrete and none on the unstained portion. I did have an outdoor carpet on the stained portion but months ago pulled it up for the winter months. I would like to put it back down but I don’t think it would be a good idea with the wet concrete. My other home did not have this problem. What is the problem here and how can I rectify it?
Elleen:
Thanks for the email. I would measure the surface temperature of the concrete in the tow areas you mentioned, see if there is any difference, and then if so compare that to the dewpoint of the air. You may be getting condensation from the air. Good luck.
I make cement candle vessels for my smalls business which is a candle company. I use a rapid set hydraulic cement. I let the cement cure for a minimum of 7 days before I seal them. I seal the 2 times with a siloxane sealer. The sealer is a breathable sealer. I have noticed some effervescence forming on a couple of the vessels but not all of them. Any advice on the why would be greatly appreciated.
Christee:
You are kind of out of my element here, but I would wager that there was a difference in the amount of water used with vessels with and without Efflorescence.
Moisture can significantly damage your decorative concrete, leading to discoloration, cracking, and efflorescence. It’s essential to monitor moisture levels and apply stains and sealers only when the concrete is sufficiently dry. Proper moisture testing, like in situ RH testing, ensures accurate moisture readings, preventing potential issues. Regular maintenance and resealing also help protect your decorative concrete from moisture-related damage, preserving its beauty and longevity.
Hello, can someone explain this to me. I soaked a carport with a concrete slab with just water. Then these white stains appeared in the concrete. They look like white paint drippings. Also a day later when the concrete started to dry a white powder formed on some of the stain. I was softwashing this house the home owner thinks I did something with my very diluted house wash mix. Can someone tell me if these stain will disappear again over time also what it is and why white powder? Thank you!
Derek:
Thanks for the question. It could be a dried “salt” from the concrete that you happened to get water on, maybe dripping from the hose? I would probably try pressure washing a small area with just water and see how it reacts. Good luck.
Our basement was flooded. Most of the floor is acid stained concrete. Each corner of the floor has whitish areas appear, from your notes above it appears to be excessive moisture.
Question….how can I remove this safely??
We have a new home with a polished concrete floor. The concrete cured for over a couple of months. It was then sealed and later it was covered with a heavy protecting cardboard paper so the carpenters could continue building and sheet rocking. Once the building was done the protective cover was removed and the floor was cleaned, sealed and burnished. White footprints mysteriously appeared after a week and could not be removed. The floor was cleaned and sealed again but now has a film blotching look and when we try to clean with warm clear water it turns white and stays the white color and cannot be now removed. The rest of the floor now has a greasy film that cannot be removed. the professional contractor than
acid washed part of the floor and resealed and burnished that part. The balance of the floor was etched and resealed… that turned blotchy and has a greasy look that will not clean off when warm water is used.
How could this be remedied so that we could again have a beautiful polished concrete floor in our new home??
Tim:
Thanks for the questions. I am having a hard time understanding the series of events and, more so, the current stay of the floor. That being said, if I understand correctly, it sounds to me that one portion was redone by a professional contractor and looks good and the other part has a blotchy look and greasy when washed? If this is correct, it seems that you need to fix the part that has a poor finish the way you did in the area that is doing well. Again, I may not understand the current state of things.
I had a new patio poured and it did not look the best so the contractor put a resurfacer on it. It has been 3 days now and there are dark and light areas. Will it ever turn all white?
Arkaa:
Thanks for the question. The best I can say is it might, and it just depends if uneven drying is causing the discoloration. Wish I could be of more help.
This is the most informative site I’ve found in my quest for ideas to fix my stained concrete floor. Thank you! My son built my house 4 years ago and we went with stained concrete floors. He’s a contractor but wasn’t really familiar with this technique. We stained and sealed the floor and it was beautiful until a white blush began appearing under the sealer in random areas. We waited about a month after the concrete was poured to stain and seal so I’m guessing there was a lot of water causing minerals to rise through the concrete. It looks awful. It’s a very small house, 800 sq ft. I want to make the white blushing less conspicuous without a major overhaul. I’m a senior with two little dogs and a cat so moving out to re-do the floor isn’t an option. Do you think if I apply another sealer then used tinted stain over the existing dark brown stain it will cover the white areas? Or any ideas you might have that I could do fairly simply would be much appreciated. I’m planning to keep the pets shut out of each area as I work on it until it’s okay for traffic so it will have to be done piecemeal.
chwhitley11
Thanks for the email. Your best bet is to consult a local specialty store that sells the sealers and stains. Explain the situation and see what their recommendations are. There may be a special wash you can use or something along those lines, but they should be able to give you some direction. Good luck.
I have recently polished the concrete in my shop. I have no vapor barrier under my slab.
Any previous effloresce I had was easily washed away.
I would like to add a “stain guard/polish” to my floor to improve light reflection and stain resistance.
Do you think any effloresce could continue to be washed away with the added stain guard.
The stain guard is a very thin water based “micro coat” that would be burnished into the concrete.
Thank you.
Jeff
Jeff:
Thanks for the question. I would say that as long as the product or process doesn’t compromise the breathability of the concrete (when you say burnish, it makes me question the impact), things should perform as they have previously. I would DEFINITELY discuss this with the “stain guard/polish” manufacturer to get their input. Good luck.
We had a new concrete driveway put down last summer. After the winter we had a portion large portion on one of the pads that had chipped and flaked off. The contractor came back out and said it was a freeze thaw issue and eventually fixed it with an overlay product. We were happy with it as it looked really good and you couldnt even tell any difference between it and the concrete. Well that was three weeks ago and yesterday after a rainstorm (the first since the overlay was applied) the entire overlay has turned a bright rust/orange color! What on earth could have caused this and what do I do from here!?
Nick:
Thanks for the question and sorry you are having problems. First, here is a link that MAY explain what is going on https://gambrick.com/what-causes-rust-stains-on-concrete/ Second, I would have an additional conversation with the concrete finisher to get their input on why and the remedy. Good luck.
I have two question regarding our new concrete
1- A new garage was built and the concrete was ground down a bit too much on one side at the garage door and it now pools when it rains and freezes if too cold. The contractor wants to add more concrete to this area to “fix it” Is that the best/only option? He offered to paint the garage floor because it will not match, but we are thinking of having an epoxy flooring added, once the issue is resolved.
2- More importantly had a new driveway, patio, and walkway done by a different company. Exposed arrogate on the boarders with a nice stamped pattern. No issues with the exposed parts, but the stamped areas have flakes that have popped up and come away from the surface. Some are 1/8″ or more deep, varying in size up to a dime size. Drive was poured in June, sealed a week or two later, now March we have all these flakes and chunks missing. Has only been 9 month, with 1 winter season. Most of the missing chunks are on the driveway, some on the walkway, with a few on the back patio. We do not use salt, only sand as he recommended, we also do not use a metal blade shovel for the snow. Any suggestions on the reason why? Also how to correct, can these be filled without having it look ugly? How can we prevent any further damages? The installer said he would re-seal again this year, he said it was salt drip off our cars, I have a hard time thinking that could be the only reason for the issue, especially after only 1 winter season. Please help if you have any suggestions.
BJ:
Thanks for the questions.
1-Uneven concrete is a very common occurrence whether in residential or commercial construction. Sometimes even the flattest floors when poured will end up uneven after the drying process. It is very common to use a “leveling” type of concrete product to fix the situation you have discussed. The only thing to make sure of is that it is intended for exterior applications, just to make sure.
2-I would research “concrete scaling”. I can’t say for sure because I am obviously not there, but after reading some articles you may have a better idea.
Good luck.
Hi We just built a basement studio with a colored concrete floor that we had sealed whennthe contractor said it was ready. Now we have the recurring white powder on the floor .It comes back even though we wipe it off. It wipes off but comes back. And then there is whiteish ” shadows ” it lookes like underneath the sealent i believe since we can’t wash it off. The studio is just finished..what to do?
Astrid:
Thanks for the question. It sounds like this is salt residue being brought to the surface by excess moisture. I would contact the contractor and have them give you alternatives. Good luck.
I read your article on how moisture can ruin decorative concrete and I realized that this is something many of my clients are dealing with. You’re so right!
The Ugly Truth: How Moisture Can Ruin Your Decorative Concrete was such an insightful post. There’s a lot of great information in it –
The type of concreate installed is smooth concreate. After a few days there was white spots everywhere that looked like it was inside the concrete. You know when you smooth concreate you go in back and forth motions, the white stuff looks like that. Nothing has worked to get rid of it. What would you suggest?
Tarman:
Thanks for the question. It sounds like these are salts coming up from the concrete as the concrete dries. I would seek out a concrete or decorative concrete store in your area. Take some pictures of the situation and I am going to bet they have some solutions. Good luck.
Hi had my crete print down over 10 years and we reseal every year and apart from a few cracks which we have repaired all is good. However I have recently had some brick work done in the garden which now needs cleaning with acid cleaner if this splashes on the crete print will it ruin it. We have yet to reseal it for this year so was going to do that after the brick work has been cleaned
Thanks
Jason –
First, from everyone on this thread…..thank you for your professionalism, depth of knowledge, willingness to say when you don’t know. Most importantly, thanks for taking the time to answer all questions…..from commercial level to simple home owner…..of which I am the latter.
I have a few spots, mostly in corners, within the house (stained concrete, dark) and the garage (foundation to slab), that are showing classic signs of efflorescence. Some just “powdery”, one spot strongly pock-marked.
Can I simply clean and seal as a mid-term solution? If so, what products would you recommend for someone with a very darkly stained floor?
Thanks!
Paul:
Thanks for the question. First, if the corners are exterior corners, I would verify that drainage and gutters around the house are functioning correctly. Second, I would recommend you contact a decorative concrete supplier to get the best product to clean and seal your specific floor. Especially if you find one local, they may be able to speak to any regionally-specific issues. Good luck.
Hi Jason
I did a renovation of a cement table top. After polishing the table top, the contractor applied some cement hardener. During the drying process, some water dripped on the table and it left a darker stain on the table top.
The contractor told me that it should fade with time when the water trapped in the cement hardener dries… What do you think?
If it does not, what is the solution to remove the stain?
Thank you!
Stanislas
Stanislas:
Thanks for the question. The contractors explanation seems plausible. If it doesn’t, you may be looking at having to “open” up the surface of the concrete to let it dry more or possibly putting a light stain on the surface. Good luck.
Hi Jason, I am having a new home built and I said to the contractor you need to make these brown rust stains disappear on this newly poured concrete floor in my garage. The builder’s supervisor said he can’t do anything about all of these stains, there are also like white calcium stains on the sidewalk and driveway as well? The builder supervisor also said after time all of this will go away when the concrete is cured fully? In your experience out in the field what can this be caused from, and what can be used by them to correct theses problems? I think this is unacceptable, your thoughts are greatly appreciated!
Thanks!
Keith:
Thanks for the questions. The brown rust stains could be high levels of iron in the water used, or from the rebar, or maybe something left on the surface during early construction. The “calcium” stains are probably salts from in the slab that are being brought to the surface. Both are fairly common and products are available to help clean both situations. Good luck.
Hello, I live in Sacramento, California and had this concrete poured in July of 2019. We noticed some dark spots in the concrete that were not drying out like the rest. I mentioned it to the contractor and they said it was common and with time it would dry.
It did not. He came out two separate times to brush it and release the moisture, to no avail. I believe this is more than discoloration but am having a harm time with the research on trapped moisture in the concrete.
Any help or suggestions you have would be greatly appreciate.
Thank you in advance for your time.
Anthony:
Thanks for the question. First, this does sound like a typical moisture discoloration issue, but I have to say I haven’t heard of anyone ever “brushing” the surface of the concrete to release moisture. I would agree with the contractor that this symptom is common and does normally go away with time. One reason you may be having a problem finding information on trapped moisture in concrete is that for the most part, excess moisture in concrete doesn’t negatively affect the concrete itself. I wish I could help more. Good luck.
Thanks for sharing such a nice article. It really helps a lot.
hello!
I used Heal and seal D2K sealer on my concrete countertop and added the powder to make it matte. The slab dried for over 3 weeks. the sealer dried for well over 24 hours and we did 2 coats. Yet a few drops of water left white spots once they dried. And i left a bottle that was humid underneath and it left a perfect white ring. It also seems to scratch easily. What happened?
Nancy:
Thanks for the question. Unfortunately, I am unfamiliar with the product you are describing here so your best bet will be to reach out to the manufacturer of the product and there technical department to determine the cause of your issues. Good luck.
As concrete contractors that do work in Florida, we know this all too well. Author knows his stuff. I learned a thing or two. Glad I found this.
I came to learn a lot of things about decorative concrete and how to maintain it! Yes, moisture can genuinely ruin the decorative. Thank you so much for sharing a bunch of suggestions. I thoroughly enjoyed the article. Please keep up the excellent work!
Yes, moisture can decrease the life of a paver. This article has helped me to understand how moisture should be prevented in order to make paver installation long lasting. Thanks for sharing this unique article.
This article provides details about how moisture can ruin decorative concrete. This blog happens to be one of the best blog, which gives proper details about it. I enjoyed reading this blog and would suggest others too, and you would get to read about it in this link.
I am doing a 3″ concrete pour and wonder about drying time. This is inside, and there is 6″ of concrete already. So 6″ concrete, a moisture barrier, 1 1/2 in rigid foam, 1/2″ pex for in floor heat, then the 3″ of new concrete. I plan to acid stay and doing it with my building contractor. Neither one of us have done this before. It is 2800 sq ft and doing in 2 day with 2 pours a day.. how smooth should concrete be finished and also once completed can I use area rugs or will they discolor the stain.
Gail:
Thanks for the questions. The drying time on the 3” pour would be about 90 days, once the environment is controlled. This is a rule of thumb. As far as a finish, most would say smooth, but not burnished. As far as the area rugs, I would imagine that if the rugs are breathable, you wouldn’t have issues. Good luck.
Jason,
I just had an outdoor patio patio poured today. They stamped in a salt rock finish. They pour around 11:30-12 in the morning and I was able to walk on it without damage by 6PM. The contractors is coming by tomorrow to apply a stain finish.
I live in Dallas, TX. It hit 90-95°F today. Question – is it too soon to have the stain applied? I asked the contractor, who I feel did a great job, about staining so soon and he said the the sealant/stain they apply is breathable and it should not be a problem. However, everything i read here tells me otherwise.
Thoughts? I hope this message finds you soon so I can make an informed decision.
Thanks!
Mike
Matt:
I would rely on the expertise of the contractor and his knowledge of the product he is using. Up to this point you say you feel he did a “great job”, I would expect that to continue.
I had concrete slab (1.5 months old) painted for basketball. About 56 hrs after the paint job was completed it rained and I noticed the there were bubbles floating in the water (some had a soapy film). What could cause that? Is there anything that I can do to rectify if this is a problem? Thoughts?
Hello, we had our contractor pour our concrete Patio in our backyard this week. There is a decorative stamped ribbon that he told us would match the stone on the house. He used an acid stain a few days after it was poured and the color turned out orange and not brown. They power washed it off and offered to add another coat but I’ve been doing a lot of reading online and worry that it hasn’t cured long enough. Will adding another coat damage the newly poured concrete? They said they wanted to seal it as well but I worry about that efflorescence. Thoughts?
Hello, I had a 4″ concrete slab poured about 6 weeks ago. It had a lou w sp ou t and tbgg e contractor added an inch or so of concrete in the low area about 5 days ago. They added concrete area is still more grey in color then the rest of the slab. I want to stain it seal it. Should I wait till the colors blend?
thank you very much
Marc:
Thanks for the question. Whether the two separate pours will completely blend in color is a big if, but I definitely wouldn’t do any finish on the slab until it has had a chance to dry further. Good luck.
We’re having an issue with efflorescence on our salon floor. The floor was pressure washed and etched, prior to spraying an acid stain to the cement. We let it set for 24 hours before we came back to check on it.. I was unable to check the entire floor because it was still wet for whatever reason, and there is also a layer of efflorescence over what appears the majority of the floor.
Where do we go from here? Can we clean the salty residue, and apply a sealer? It’s not quite as dark as we like so we planned to apply another coat of stain, but is that from the efflorescence? This is our first floor we’ve ever done. Thank you!
Kyle:
Thanks for the questions. If the residue is efflorescence it is a salt that has traveled within moisture from the slab, to the surface, and dried. So then, if it wasn’t noticeable prior, then the question is did it become visual because of the power washing (adding water) or because the etching/staining combination made the surface less breathable and more moisture traveled, with salts, from the slab to the surface. The lighter areas may be a sign of higher than desire moisture causing the color pigment to dilute. This may be moisture in the concrete or the power washing. Understanding the moisture condition of the floor would be a great first step. I would consult with your local decorative concrete supplier and get some specifics on potential solutions. Good luck.
I have a large, stamped, colored concrete porch which is several years old. It was sealed when it was first done, but hasn’t been sealed since. Part of the reason is that there are hard mineral deposits where I have had large planters. Over time the deposits
have spread and gotten worse. I’ve tried different things to try to remove the buildup, but nothing seems to help. Can you???
Debra:
Thank you for the question. I can’t give you a product recommendation, but I can give some advice. I would find a supply house in your area that specializes in decorative concrete and explain the situation to them. They should be able to give you guidance on a product that might be the most effective in your situation.
Moved into our new home in December and unfortunately seems as though our contractor rushed the concrete work which has resulted in white discoloration on the walkway (don’t think it’s Efflorescence, just from the tarp getting covered in rain water).
As far as the concrete near our house it has small white cracks along the border.
Would some sort of acid cleaner and sealant improve the look? I know the contractor won’t redo the job, but I’m hoping to pressure them to do something as every other house in the neighborhood has a clean finish. I’m assuming power washing won’t accomplish anything.
Photos: http://imgur.com/gallery/46qu3fF
Colin:
Thanks for the question. I would imagine that the first step of any process here will be pressure washing. Prior to that though I would consult a concrete sundry distributor in your area, explain the situation, and seek specific guidance and potential product recommendations. Good luck.
Hi,
We had a stamped patio installed a few years ago in August. The following spring, it had a bunch of blisters, and flaking. The contractor came back out, resurfaced and restained and sealed in April (we live in southern Maine). Now that the snow has thawed from winter, we see more blistering and peeling. Less than before, but it is happening again. Is there something we can do to stop the blistering and peeling and prevent future continuation of this?
Jennifer:
Thanks for the question. I would have a very pointed conversation with the original contractor to get a better understanding of the cause. I have found that doing so without any notion of getting something redone tends to get better results. From what you said the second application has better results so did they change product, do better preparation of the surface, etc. These are the things to find out and then use to map out your next steps. Good luck.
It’s helpful that dark spots are a sign of moisture that can’t evaporate because that’ll help me solve the problem should it arise. Our current deck has a huge grease spot on it and it’s looking worse for wear so we’re getting a new one. My wife thinks that decorative cement will look really cool! I’ll be sure to be careful about moisture when we get it installed.
Hi Jason. My stand-alone garage sits at the lowest portion of my down-sloping lot. It was built in the 1970’s, before I owned the property. Sometimes during the rainy season we get some moisture on the floor, which I assume is coming up through the concrete slab. in those spots the epoxy finish has peeled away. Assuming I do not want to replace the slab, can I replace the epoxy with any kind of finish that can withstand the moisture? If so, what? Or should I just have the epoxy sandblasted off and call it a day? Thanks.
Grouper:
Thanks for the question. There may be more moisture resistant epoxy products out there for this application. I would do some research on coatings looking specifically at the moisture side of the equation. Calling some of the bigger manufacturers technical departments and explaining the situation may also yield great insight. Good luck.
Hi Jason. I’ve solid stained my patio and it already has bubbles popping up. I don’t want to make the same mistake with my porch and walkway. Wondering if there are any issues with bubbling with water based semitransparent stain and what brand is recommended as I’ve read some horrible reviews on the big store brands. thanks!
Jenn:
Thanks for the question. We try not to get into specific manufacturer’s products, but it the reviews aren’t good for the type of retail establishment you are speaking about, I would look to find a business that specializes in paints and coating. Makes sure the porch and walkway surfaces are completely clean and make sure to follow, whichever manufacturer’s product you use, surface preparation instructions. Preparation will make or break a project.
Help!
I recently made a concrete garden bench with powder color added to the mix and also used a concrete stain paint once dried to color in the grape design. I let the bench cure for about 48 hours before staining the grape design with color stains then sealed with a water based glaze and sealer… Two coats every 24 hours… The bench looked great until it rained, now the color design stain has been washed away by 50% and the bench looks bleached.. Before it was a light beige color… What could have happened? I’m in Ca and the weather was around 70 when making….Thanks Karen
Karen:
Thanks for the questions, but I am not sure how much help I will be. It sounds like the “color” just didn’t absorb into the concrete at all and may have something to do with the concrete itself and the amount of time (or lack thereof) that the concrete was allowed to cure and/or dry. I would consult the manufacturers of the products you used on the bench and see if they can shed light on the issue. Good luck.
What a great service you’re providing to people. Thank you! My 85 year old neighbor had a new concrete porch and walk poured in the late fall. (Our management provided it, via outside contractors. They covered all of it with plastic to dry, because a cold snap was approaching. When it dried, it had dark lines/patterns all over it. It looks terrible. The contractor was just here today with chemical treatments that didn’t work. He left to look for other products to try. He doesn’t know if anything will help, but says it should fade with sun and weather “over the years”.
What caused this, and is there really no solution except “years”? I’d love to help her with this. She has such a lovely yard and is understandably upset with the way this looks. It’s a large porch and walk, very new and white, and the stain patterns almost black. I’d be glad to work on it with a deck brush if I knew what to use.
Again, thank you for your time and expertise.
Clueless:
Thanks for the question. These lines could just be areas where the concrete is still wetter than the other areas, its hard to say from your description. If it is really that bad, they may want to look at some topically applied colorant for the concrete to mask the issue. A decorative concrete contractor may be able to help. Good luck.
Hi,
I recently had my concrete sealed for its 3rd time after 10 years, The first time the colour was similar to the coloured concrete, the last 2 times was a change to black.
Before having this change we noticed after rain that we would be left with white powder around the the cuts in the concrete where water would seep up and then disappear.
After having the new black colour it didnt take long before the black peeled off in patches and to clean the concrete with a hose would remove the paint.
I had the tradesman come back to repaint and he said he was unsure if it would happen again…. It did… 1 month later the paint has peeled off again in the same areas.
What are we doing wrong and how do we fix it?
Dan:
Thanks for the question. It sounds as if it may be a moisture and/or a surface profile issue. I am not recommending any products specifically, but this company gives some good visuals and potential remedies. Good luck. https://www.sherwin-williams.com/homeowners/how-to/problem-solver/peeling-cracking
I have a question. My basement flooded and our floors have been stained and beautiful for two years. The water made it bubble and peel up. Do I sand it down, stain again and top coat it again. What grade sandpaper would I use if this is a fix.
Stephanie:
Thanks for the question. You may have to do all of these steps, but the finish coat may just need to be removed and another finish coat of applied. I would contact a decorative coating supplier in your area for specific recommendations. Good luck.
Every concrete contractor needs to have this information, so stamped concrete can start getting a better reputation! It’s sad that people have heard so many bad things about stamped concrete, when all that needs to happen is contractors to have better skills and know how to make that stuff last! Thanks for sharing this scientific info!
I bought my house brand new two years ago. about 8 months into living in the house. My floors are light color stained concrete with design grout throughout. I live in texas and all houses are lined up. So pretty much was land and now houses all the same lined up from street to street. When it rains a crack in the front entry way gets dark spots, moisture in them and stays like that until it dries up. Since it has been a rainy season we have not caught a break. There are now water stains big water stains, noticeable where the water dark spots are. It happens every time it rains. i got gutters put on the house and also had the roof inspected and the crack outside the door resealed. The crack that the moisture comes up isn’t big to where my inspector of the house finds it alarming. There are natural cracks through out the house. The front entry way is the only area where it is pretty much ruined. Terrible water stains and dark spots until they dry up which some times is weeks if not a month. I do not what or if there is anything I can do.
Kerrie Desai
Kerrie:
Thanks for the questions. I would first focus on ensuring there is proper drainage away from the house. Having gutters doesn’t always ensure the water being diverted to the downspouts is making its way away from the house. That being ensured, I would question if there is an intact vapor retarder below the slab. To verify that, if this problem is substantial enough to you, you may need to consult with someone to do core samples of the slab. Good luck.
Jason – it appears you have no shortage of problems! I have a newly laid exposed aggregate driveway. I initially applied 2 coats of solvent sealer, the first diluted with solvent as per manufacturer recommendation and the second undiluted. The sealer dried and looked good. A few days after rain, the concrete had a spotted appearance (the area under cover and not rained on was OK). On closer inspection it appeared that the sealer had not penertrated into all the small pores in the aggregate and the water was ‘wetting’ these areas. On advice, I applied another coat (undiluted) – this was after a suitable drying time and the wet spots had disappeared. Alas, after rain the spots are back again as if the sealer had still not penetrated all the pores. Should I try to apply another undiluted coat or a diluted coat (less viscous) to try to fill these pores??
Leigh:
Thanks for the question. It seems, based on your observations, that the sealer isn’t penetrating, or getting into the pores, is certain areas. I would be trying to find the appropriate solution for this symptom. Contacting the sealer manufacturers technical line would be my first phone call. With some discussion and possibly a few photos they should be able to line things out. Good luck.
Jason
I have a dark stain on concert that I found under stained carpet it is a rental I think it could be cooking oil also how can I tell
Tonia:
Thanks for the question. The best I can recommend is that you put some water on the dark area and see if it beads up. This will at least potentially tell you whether it is some type of oil based product. Good Luck.
Jason
Hi Jason – appreciated this article and think I am dealing with moisture issues. We just had a new concrete floor poured in our home. The contractor applied a sealer over the integral concrete. Dark spots have begun appearing randomly, as well as some long surface cracks, uneven coloring, and noticeable blistering. Our contractor is proposing that they sand down the surface to remove the seal, let the concrete breathe, and then reseal the concrete when it is suffiently dry. Does this seem like a reasonable approach? They are proposing sanding with hand-held units and I am concerned they do it unevenly. Also, will the moisure-based discoloration disappear if the seal is removed? Appreciate your thoughts and I have photos to show it helpful.
Mike:
Thanks for the question. The contractor’s approach seems valid, although the hand-held units seem like it would be fairly labor intensive. As far as the discoloration, in theory, it should dissipate, but that isn’t always the case. My only question about the process would be, once the concrete has been deemed properly dry, what additional concrete preparation steps will be necessary prior to sealing the floor? It would seem to me, if the floor is “opened” up, if foot traffic happens on it for say months, the concrete would need additional prep prior to sealing. Just a question to ask.
I agree it does sound like efflorescence. You should have a tradesman look at it to confirm. If it is there isn’t anything you can do at this point except remove the sealer/coating put a vapor barrier on it and reapply coating. You can try to clean the efflorescence off with vinegar (cut 50/50) and a soft bristle broom. Efflorescence is more noticeable in winter than summer.
Jason, I work in a building that was built in the 60’s with no vapor barrier. When the building was upgraded about 10 years ago they used vinyl tiles on the floor. As you can imagine the adhesive didn’t hold and now the tiles are peeling up. We’ve had flooding people come out and they have measured the moisture content in the floor at about 80% (We are in Florida). What is the best solution for flooring in this case?
Amy:
Thanks for the question. In the scheme of things, 80% RH, in most cases, is a great number for installing finishes. Unfortunately, that number for you is really inaccurate because you know there is no vapor retarder under the slab. What that means is that the 80% RH today could easily increase to substantially higher RH% if the moisture vapor in the soil increases because there is no separation between the soil and the bottom of the slab. You could either try for a more moisture resistant and/or breathable floor covering or apply a moisture remediation product, good to 100%RH (make sure the product warrants even if the slab has no vapor retarder) to the surface of the concrete. Most other options would be done knowing continuous repairs were going to be necessary to keep the floor in one piece. Good luck.
Jason
Our exposed concrete is 4 years old. It has a clear solvent glaze applied when new. We have redone it again but it has gone white under the stain. When it was done it looked fantastic. The contractor doesn’t understand what went wrong and has no answer to correct this .. can you help. The area is over 200/m2 Thanks David
Thanks for the question. It sounds as if salts have migrated through the slab, to the surface. Sometimes when finishes are redone or changed, the breathability of the concrete is altered. With many breathable finishes, the moisture in the slab can travel through and into the air, never leaving behind a noticeable salt residue. If the new finish is applied and it is less breathable than the previous finish, it may leave this type of whitish stain. Obviously, you may also need to look at any potential product issues. Good luck.
I recently had my concrete floors polished, stained and sealed. The problem we are finding is that there are yellow blotches on our gray floor. We had VCT that were removed and the mastic cleaned away. The yellow spotting only occurs in the areas where there were tiles. When we put down the stain the spots are not visible but when we sealed the floor they would show up. Is there anything we can do?
Thanks,
Danny
Danny:
Thanks for the question. I would get back together with the contractor and have this discussion to see if they have seen this issue prior. It could be the lack of breathability of the sealer, residue left from adhesive removal, etc. Having this discussion should allow for an appropriate plan to be established.
Thanks,
Jason
It really is such a science if you think about it! It so interesting to me how different levels of moisture, temperature, and other variables can make such a difference! That is why when somebody tells you about a bad experience that had with certain types of concrete, you can’t always just go with what they said because who knows what kind of circumstances their concrete was poured. Great article on how it all works! : )
You describe a problem above that I am experiencing, my blue stamped concrete has turned mostly brown. This happened after an application of sealant. I had been resealing it every 2 years prior to that with no problems. Is there a fix to this problem or am I stuck with the brown?
Patti:
Thanks for the question. Depending on what exactly has caused the problem, you may be able to have color reapplied topically to restore the previous appearance. I would have a decorative concrete professional come out and take a look. Good luck.
Thanks,
Jason
Since I’m always on the lookout for more concrete knowledge, I was very pleased to come across this wonderful info! It got me really thinking and also lead me to make sure all of my guys were waiting the right amount of time before adding stain and sealer. Thanks for the reminder!! : )
I have an outdoor fire pit that is supposed to be made of cement. The entire top is bubbled up and cracking really bad. The cracks are slowly creeping down the side. I was wondering if it would be possible to hammer the bubbles out, remove the cement to the metal surface, fill in with an adhesive and tile over the metal? It’s really heavy and only 6 months old. We have no way of removing it but it looks horrible. Our son wants to get married in our back yard and I don’t want the fire pit to take away from the look of the patio area. Thank you so much.
Cindy:
Thanks for the comment. Your question is very specific to your situation and not a common one I have received. That being said, I can’t say whether your proposed solution would work. It sounds like it could be viable, but I wouldn’t know for sure. Good luck.
Regards,
Jason
Thank you.
I have had a cream polish done on a new slab, it was fully cured and dry, we covered with chipboard after the cream polish to protect during construction period and rain got in, areas have milky white bubbles apeard, and some of them the coating scratches off with fingernail, concrete polisher claims this is my fault because moisture got trapped and charging extra to fix it.
does this sound right ?
Simon,
Thanks for the question. Depending on the breathability of the chipboard, he may be correct. The moisture can get trapped and cause issues. The only way to really know is if you have an independent inspector or possibly the supplier/manufacturer of the products used in the polishing. Good luck.
Jason
Jason
I’m in Florida. We have an undercover concrete patio from the 1980s that was covered with outdoor carpet until 3 years ago. Our contractor removed the carpet, ground the surface, laid a textured layer, stained it and then clearcoated it. It looked fantastic but within a year white blush appeared in some areas below the clearcoat. The contractor removed the clearcoat and laid on one that was supposedly a little more porous but the problem came back and is now extensive. It seems to be efflorescence. The only other fix they have tried is to brush xylene on the affected areas. It helps a bit but does not completely remove the white and soon the white returns anyway. They tell me that they are now are out of ideas.
Is there some kind of epoxy paint that I can apply that will hold the efflorescence blow the color layer or some other such solution, please?
David:
Thanks for the question. Here are some good tips from the Portland Cement Association: http://www.cement.org/docs/default-source/fc_mat-app_pdfs/masonry/is239-pca-efflorescence.pdf
Make sure to read to the end for decorative concrete. Good Luck.
Jason
Hi Jason,
We had our polished concrete floor done in our lower level of our home (which is below grade) about 4 years ago. We have been dealing with a “stale” smell in our home ever since. We have done everything imagineable to rid the smell and have had mold testing done twice (which both came back negative). I recently had a an odor remediation specialist come in a few months ago and he said he thought the smell had a “building materials” smell to it. He was the first person to point to the concrete as a possibility. Our house is an open concept so the lower level is open to the rest of the home. And we just recently installed a whole home dehumidifier to help with moisture levels in the home. Today I went downstairs to do some more investigating the lifted some carpet tile area rugs and realized that the concrete under the rugs is discolored. This led me to a google search and to your post. Do you think a unproperly sealed concrete could create the smell problem and the discoloration? Thanks for your guidance
Anne:
Thank you for the comment. While I haven’t ever heard of concrete moisture directly causing odor, the discoloration underneath the rugs might be indicative of excessive concrete moisture. You may need to have someone out, possibly an engineer, to evaluate whether there is an intact vapor retarder under the slab and what levels of moisture are in the slab. FYI, in order to verify the presence of a vaper retarder, they will have to do core samples of the slab, but knowing this helps to understand whether moisture vapor is being allowed to enter the slab through the soil. You may be able to also send the core sample out for analysis to see if that can help shed any light. Good luck.
Hi Jason
Is there anywayay of staining old house floors that are consistently damp. No barrier was placed under conctete. What I need is a sealer that can breath and release moisture…..
Thank you
Phil
Phil:
Thanks for the comment. Yes, there should be options for you in this situation. My best recommendation is to contact a reputable decorative concrete contractor in your area. Good luck.
Thank you!
Jason
Hi
I poured concrete . I wanted a white screed finish . Today my floor had lots of cracks and my screed is turning brown in some areas. Please advis
Doreen:
Thanks for the comments. The surface cracking usually has to do with the early drying of the concrete. i.e. dried too fast, not enough surface moisture kept in, for long enough to help with early curing. As far as the color, the best I can say is the “brown” areas may just be areas with more moisture and, when they dry, the color may lighten.
Jason
We had our 16 year old driveway resurfaced and stained last January. There is a large area that never dries out and appears to be condensing moisture in the air. The driveway is wet to the point where there is a small puddle in this area. The sealer is bubbling up, flaking and peeling in the wet area. Underneath the flakes of sealer, the concrete looks wet. It appears that the moisture is coming up from underneath the driveway. The driveway has been restained several times, but it doesn’t seem to adhere in the wet area. The remainder of the driveway that isn’t wet has a very nice appearance.
Would waiting for the hot summer to dry it out would that permit me to recoat the wet area and have a chance of holding up?
thanks
Chip:
Thanks for the question. It may help the sealer better adhere to the top of the concrete, but obviously, it doesn’t sound like it will keep the moisture from coming to the surface. I would find a knowledgeable supplier of sealers and have a discussion with them regarding best material type sealer to use for this situation. This may require a chemical makeup different than the sealer on the rest of the concrete.
Thanks,
Jason
Last November we finished building two new homes on the same lot. The bottom floor, for both, have finished concrete with radiant heating pipes thru it. We applied the finish decorative stain and sealer six months after pouring the original slab, so plenty of time to dry. (it was the summer in California) We used two different colors on each, one was antique gray and the other dark chocolate. Now, one year later, the house that had the dark chocolate starts to show problems with the finish. If you walk bare foot, you would get brown bottoms, in one place, under a area rug that had the rubber pad under the rug for movement, that rubber completely sticked to the floor and looked like its melting. In some area it’s even cheeping like paint.
The house that had the antique gray applied has no issues at all.
What do you think is the issue and how can we fix it?
Hortensia:
Thanks for the comment. There could be a number of issues. The rubber on the rug makes that area non-breathable and it could be causing more moisture and more salts to migrate from within the slab; raising the pH at the surface. The breathability of the two applications may be different. Application techniques could have varied from one job to the next. I would have either the original applicator or someone else within that trade come out and assess the situation. I hope this helps.
Jason
I’m looking into finishing the concrete floor of a 1,200 sq ft 3 car garage/workshop. I’ve looked into epoxy and stain options and both paths appear to have limitations and degradation concerns around scenarios where you have excessive moisture issues. The structure is built on a hill/slope, at the end of a larger hill and the area has a high water table. Not sure there was an actual water vapor barrier under the slab either. Let’s just say long term, there is no real way to effectively mitigate the excessive moisture issues as a whole that would negatively impact concrete floor finishing applications.
Are there any options that would work best considering this ongoing high moisture scenario?
Adam:
Thanks for the comment. I would look for a very breathable coating and/or look to just doing a polished natural application with a sealer. Either way, I would consult a coating/polishing professional in your area for guidance, whether an actual contractor who will be performing the work or a knowledgeable supply house that can offer advice. I hope this helps.
Thanks,
Jason
I moved into a rental that has very dark stained concrete floors. Per the rental agreement we are only allowed to use Bona floor cleaner and water on the floors and they require the floors to be refinished every 6 months. I have complied with the maintenance of the floors and last finished the floors in August. I have been noticing rust colored spots ALL over the floors, and even under the rugs and behind the fridge where no finish was applied. It’s all over; the beautiful dark maple finish is now spotted everywhere. I’ve also notice blistering of the floors in certain areas and a milky color in some areas well. It seems to be getting worse and I’m not sure what to do. The house in about 3 years old, I’ve lived here for about 8 months and I believe they are going to try to charge me for the floors because I was told that they didn’t have this problem when they lived here and the previous tenant did not either. What can be causing this on the floors? Was it a problem when the cement was poured? Stained? Why is it just showing up now? I’ve asked them to ask their builder who informed them if the floors were maintained there should be no discoloration, but I’ve only used a neutral Bona cleaner and steam mop in between cleanings. Help.
Ange:
Thanks for the question. It’s hard to say exactly what the issue is here. It could be that there is no vapor retarder below the slab. With this, depending on the amount of moisture in the soil, the potential for “issues” on the surface may vary. This may be one reason for your “why now?” question. Another thing could be the refinish…was it done by the same people that have done it the last three years? Was the same product utilized? These are a couple of things that may potentially cause the issues you are describing. Good luck.
Jason
We had our slab poured in the summer of 2016 and the shop/apartment went up over the winter. This spring we laid laminate flooring directly on the slab. A few days later we noticed they were peeling up due to moisture. We had a very hot, dry summer but trenched all the way around the house to make sure that wasn’t the issue. Recently we had someone do a decorative stain and seal on the floor. About one month after it was down we noticed blistering on the floor. There has been no discoloration but the blistering encompasses most of the 1400 basement. We were told the vapor lock that was applied would eliminate any moisture from surfacing. Any idea if this is true or if we are looking at another moisture issue?
Dianna:
Thanks for the question. Obviously, without being there, I can’t be sure, but it sounds like another moisture issue. Not all “vapor lock” type products work on unlimited moisture levels, so testing is necessary to apply the appropriate product. I am not sure if they tested or not, but this should be one of the first steps.
Thanks,
Jason
Our stamped concrete is four years old and the first coat of sealer that was applied at the time it was done was fine and looked great but after a couple of years it was looking dull. We decided to put another coat of sealer on it last summer, it looked great all summer but over the winter a good portion of it now has white areas either under or in-bedded in the sealer. How can we fix this? Can it be fixed without stripping it down to the concrete?
Rhonda:
Thanks for the comment. I would reach out to a local decorative concrete contractor to diagnose the problem in order to come up with a proper solution. You may need to, as you suggest, start from bare concrete in order to “fix” the problem and then apply a new topping/sealer, but there may be a better alternative that they can recommend.
Thanks,
Jason
I had a new patio poured and it did not look the best so the contractor put a resurfacer on it. It has been 3 days now and there are dark and light areas. Will it ever turn all white?
Jim:
Thanks for the question. It’s hard to say for sure, but as concrete cures and dries it will usually develop one, fairly consistent color.
Thanks,
Jason
August 12, 2017
Dear Jason,
My brother In laws, hubby and myself decided to add outdoor tiles on top of an existing concrete patio slab. We are not professionals in anyway, but have helped to complete many other outside garden projects together like pergolas and such. My question is: after we put down the tiles, the rains came and we covered it with a tarp for several days — so not to get them wet as they were drying. That was over the 4th of July weekend. We have been getting rain almost every day/week as to date. When we waited the 10 days prior to lift off the cover tarp, we saw white residue and when we stepped on it, it oozed and bubbled in certain places. I know this is too much moisture underneath. Now what do we do? We can’t stain it yet, because everyday it’s raining again and now it’s uncovered as it just sits. I can even press down the grout with my finger between the connecting tiles–cause it’s soft. We tried to do this by ourselves to save on a professional coming in, and ironically it looks rather nice with its slate stone finish. But still, I believe even if the professionals did come, they and we still would have had the same problem because of this endless rain almost every day.
The backyard patio is not a big area- just an average step-out length rectangular area, but what do we do now? Should we pull the whole thing up again and have someone else do it or what? This rain is not letting up on the weekends or some weekdays. My brother in laws went back to Ohio.
We live in Tampa Florida by ourselves and me and hubby can’t do this project alone.
Rita:
Sorry for the problems. First, I am not sure what kind of setting material you used. If it is a Portland cement based mortar, I would think the 10 days of tarping should have been sufficient for the mortar to set up. It sounds as if the mortar may have been severely over watered at placement and/or the tarp did little to nothing keeping the rain out. I would think, depending on the severity of this issue, that the mortar will set, eventually, but with so much water, the bonding strength may be compromised. I would contact the manufacturer of the setting material and have a discussion with them prior to doing anything drastic. I hope this helps.
Jason
I just moved into a brand new home with a water-based acrylic stain throughout the house. The stain is peeling/flaking up with the most minor of abrasions. For example, had to put the brand new fridge on the ground and roll it into the refrigerator cabinet..it dug through the finish and down to the bare concrete. Under our bed frame where the roller shifts around slightly, there are flakes coming up everywhere.
What did the contractor do incorrectly? How can it be remedied?
Thanks,
Austin
What is the long term prognosis for a concrete floor which has multiple paler llemishes appearing below the sealer.
The floor has been done now for nearly 12 months and getting worse. Is it a problem the tradesperson should be fixing or is it just bad luck. I am worried there will be total long term deterioration..
Sharon:
This is hard to diagnose via email. I would start by enlisting the tradesperson that did the work and get their professional opinion.
Jason
If a stain is already flaking/chipping as a result of a high RH in the slab prior to sealing would the introduction of water to the surface exacerbate the problem? For example if a large amount of water from a failed plumbing supply line pooled on the floor could that water migrate into the slab and then result in the stain chipping? Thank you in advance for your response.
Lance:
Thanks for the question. It’s a possibility. The flaking could make the surface of the concrete more permeable, allowing additional moisture into the concrete. The problem may also stay somewhat localized if the intact portion of the “system” has low permeability and doesn’t allow much of the moisture past the surface.
Thanks,
Jason
Excess moisture doesn’t just evaporate; it takes your design with it. You can preserve your design and the concrete with proper moisture testing before stains and sealers are applied. Beauty and strength converge in decorative concrete. Like a good acid stain, they fuse together to create a durable, pleasing floor that literally becomes the foundation of its space and atmosphere.
I think my concrete guy applied the sealer before the concrete was dry enough. It looked fina at first, but now several days later there is a white film under the sealer. Is there a way to fix this? This was supposed to be my finished floor in my new house, but now I don’t know what to do. Thanks for any info you can provide. Jack.
Unfortunately, the description you provided could be multiple things. We could be talking efflorescence, which is the salts migrating up through the concrete. This could potentially be under the “sealer” or on top of it. The salts are always available in the concrete, but usually high levels of moisture can act as the vehicle, transporting them to the surface. There could also be an issue with the “sealer” itself. Remedies for either could be different. As I will always recommend, go back to the tradesperson who did the work and see if you can come up with an appropriate remedy.
Jason