Why Measure Moisture in Old Concrete Floor Slabs?
Here’s a pop quiz for all of you flooring installers.
You’ve got a 30, maybe 40-year-old concrete slab that “looks and feels” dry. Is it dry enough to install new flooring and coating materials?
Before you answer, consider this . . . concrete slabs on ground poured 30 or 40 years ago probably didn’t have a proper vapor retarder installed.
And if a proper vapor retarder was installed, it has likely deteriorated and may no longer provide adequate moisture protection below the slab.
In this case, unless you install a moisture control system on top of the slab, moisture may be able to move to the slab’s surface, potentially leading to serious problems; even floor covering failures.
That’s why it’s always imperative that you take the time to assess a slab’s current moisture condition — even the old, supposedly dry, slabs.

Older concrete is not always dry enough to ensure a successful floor installation.
In fact, it’s estimated that moisture-related flooring problems cost contractors, installers, manufacturers, and property owners an estimated $1 billion annually because of call-backs, repairs, and disputes.
Now back to our pop quiz question — is a 30 or 40-year-old concrete slab that’s dry to the touch also dry enough to install new flooring and coating? The correct answer: Not necessarily.
Two common misconceptions about old concrete slabs can lead to serious moisture-related flooring problems. It’s often believed that:
- If a concrete slab is “old,” that is, one year or older, it’s sufficiently dry for installation.
- If the slab’s surface feels and looks dry, it’s ready for an install.
Unfortunately, an “old” concrete slab or one that appears “dry” can be deceptive.
Misconception #1: Old Concrete Must Be “Dry”
In the case of old concrete, if it’s already had flooring installed over it, it seems logical that it must be dry enough for new flooring.
Wrong!
Older flooring systems often used products that were more moisture-resistant than many of the products used today, but also typically had a greater environmental impact. This means that an old concrete slab may be retaining moisture that was sealed by the older, more moisture-resistant flooring.
Although this moisture may not have harmed the older flooring, it could certainly damage new flooring that’s not as moisture resistant. For these reasons, never assume an older slab is sufficiently dry for a new flooring installation.
Moisture-related flooring problems have always plagued the industry. However, as formulations began to change for specific applications, it has become increasingly important to ensure that concrete slabs under the flooring installations are sufficiently dry to prevent moisture-related problems later.
With the more recent focus toward lowering VOCs (volatile organic compounds) in products used in the construction industry, today’s flooring products and adhesives can vary greatly in their tolerances to elevated moisture conditions.
For best results, always evaluate the slab’s moisture condition before proceeding with any flooring installation. Installers should also be certain the product specified is compatible with the slab’s moisture condition.
If it’s not, then consider choosing products that meet the current moisture condition of the slab. If opting for a different flooring product is not feasible, then prior to the installation, be sure to apply a sealer that’s compatible with the finished floor product.
Waiting for the concrete to dry is probably not a viable option because an older slab usually won’t have a properly working vapor retarder

Free Download – 4 Reasons Why Your Concrete Is Taking Forever to Dry
Misconception #2: The Surface Appears “Dry”
What about an older concrete slab whose surface appears completely dry? In this case, an installer may believe this gives him the green light to proceed with an install.
Again, wrong!
Studies have shown that the dryness at the surface of a concrete slab won’t necessarily reflect the slab’s overall moisture condition. Ambient conditions around the slab, such as temperature, humidity, and airflow, can cause the slab’s surface condition to be very different from what’s going on below, where it matters most.
In addition, after old flooring is removed, moisture that’s been trapped in the old slab will begin moving to the surface and evaporate. Once this happens, a moisture gradient invariably forms so that the moisture condition deeper within becomes different than at the surface.
Therefore, a concrete moisture test that only measures conditions at the surface, such as with a moisture meter or the widely used anhydrous calcium chloride test, is potentially risky.
While these tests may accurately describe moisture conditions at the surface, they fail to reveal the slab’s overall moisture condition — especially moisture deep within the slab. And that can lead to serious problems.
Consider the surface tests just mentioned:
- Moisture meters, while a useful survey tool, typically operate at about ¾” depth and can be susceptible to rebar, aggregates, and more within the slab.
- The calcium chloride test (or MVER) has been shown to measure moisture conditions in the top ¾ inches of the slab only.
No surface test tells an installer how much moisture is present deeper within the concrete – which is critically important, as that moisture gradient will equalize if a non-permeable floor covering is installed. Scientific studies have shown that surface tests often give readings that are not indicative of the slab’s overall moisture condition.
Science-Backed Testing
Assuming for the moment that the slab actually has an intact vapor retarder, we know for the long-term performance of any floor, what really matters is the slab’s point of moisture equilibrium. This occurs after flooring is installed, when moisture can no longer evaporate from the slab’s surface.
The existing moisture gradient from top to bottom then tends to even out, creating an equilibrium and a moisture condition at the slab’s surface that may be very different than at the time the flooring was installed. This is the actual moisture condition that the installed flooring will “see” for the long haul.
With this in mind, it has been demonstrated that the only way to get an accurate, reliable assessment of this “true” overall moisture condition in older concrete is by taking moisture measurements at specific depths – 40% depth for a slab drying from one side, and 20% depth for a slab drying from two sides.

This is what in situ relative humidity (RH) testing is specifically designed to do. RH testing performed according to the ASTM F2170 standard is based on modern science and engineering principles. It’s also fast and affordable.
Now if the RH numbers were to come back high, indicating that the concrete is too wet for a successful floor installation, the question, of course, would be why? Does the slab lack an intact vapor retarder? Most likely, the answer is yes, although taking core samples would address this question for sure.
The best approach may simply be to apply a sealer on the concrete to mitigate for the slab’s unsuitable moisture condition.
Flooring contractors should always remember: When preparing to install any type of flooring over an old or seemingly “dry” concrete floor, don’t assume that the concrete is actually dry enough for a successful installation with today’s flooring products.
First, conduct an in situ RH test. It’s the only proven test method giving consistent, reliable information about the slab’s overall moisture condition.
This article was originally published by The Flooring Contractor in the Winter 2017 issue.
Jason has 20+ years’ experience in sales and sales management in a spectrum of industries and has successfully launched a variety of products to the market, including the original Rapid RH® concrete moisture tests. He currently works with Wagner Meters as our Rapid RH® product sales manager.
Last updated on February 16th, 2024


This does not answer the question of what will happen long term. You could test and find no moisture, but isn’t the test good for only the day it is taken and could fluctuate weeks from the test after a change in weather due to the barrier being compromised? In this case, you would install knowing you have a dry slab that day, but have the customer complaining of glue pumping up through the seams a year and a huge storm later? That’s the big question…..do you move forward with installing a hard flooring in an older building where there could be moisture problems without spending a fortune on barriers? Do you push back when your customer wants a test? I’ll do the test, but how long is it good (in an older building). I have your pinless meter for wood and concrete is this a reliable method for concrete slabs?
Does the RH test tell me something about the history in some way?
Thank you.
Sarah:
Thanks for the question. One of my big things is that business owners will always have some level of risk in order to be in business. Level of risk tolerance is an individual choice. If you want little to no risk tolerance in an older slab installation, you would do a core sample to validate if the retarder is intact and if so, moisture test the concrete to find an installation path forward. If you core sample and there is no intact retarder or if you don’t core sample and just assume there is no vapor retarder then you need to find a “gold standard” moisture mitigation product that doesn’t have exclusions in the warranty regarding “no vapor retarder present”. Now, most have told me that if they did this, especially in the retail environment, they probably would go out of business.
On the other end of the risk spectrum is doing nothing and just installing the floor which would probably also cause someone to go out of business due to flooring failures. So, what most will do is chose and industry acceptable method for moisture testing, either RH or CaCl2, and make a decision based on that. Is it perfect, no. Is it lessening your risk, yes.
“do you move forward with installing a hard flooring in an older building where there could be moisture problems without spending a fortune on barriers?” The answer is it depends on your level of risk tolerance and you should always do tests, unless you are planning on using that “gold standard” moisture mitigation product.
Our concrete meters is as reliable as any non invasive concrete meter out there, but very few manufacturers recognize that type of testing to make an installation decision. That being said, especially in the retail world, we have many installers that use it for that.
I hope this helps.
Really helpful to know these tips! Its hard to find the right steps to take. Thanks for sharing!
I’d like to start performing this technique not only in basements, but also garages. I know you see these problems arise in some garage floors, especially when the driveway slopes down hill the garage is attached to the house.
Thank you for your information.
I am about to take up a tiled floor over a slab 4 years old and replace it with a hybrid floor laid on ply(for height).
Therefore from your information I guess I should use a moisture barrier over the slab.
What about a 30 to 40 year old elevated concrete slab? (i.e. not a slab on grade)…
Pat:
Thanks for the comment. There is nowhere in flooring installation documents that I have seen that excludes old, elevated slabs. Slabs may have been covered up, way back when, with products that withstood higher levels of moisture. These floors, in essence, may trap the moisture in the slab and when you demo and install without moisture testing, you may be uncovering a beast. This would be especially true with slabs poured in steel pan decking.
It really helps to know these tips ahead of time before hiring someone for a fix! That way you are more aware of the steps and the way it all works! Thanks for sharing this helpful info!!
had floorting installed 2yrs ago and removed for replactment and mold around outer wall